Road Construction Bitumen 40-50 Petro toloe Jam

Density

٠٦/١-٠١/١

Penetration Rate at 25C

٤٠-٥٠

Softening Point ºC

٥٢-٦٠

Ductility 25C (cm)

Min 100

Flash PointºC

Min250

Solubility Disulfide %wt.

5/99

Stain Test

Negative

Wieght Loss by Heating %wt.

Max 2 /0

Wieght Loss by Heating، %

Max20

Road Construction Bitumen 40-50 Tejarat Aftab

Density

٠٦/١-٠١/١

Penetration Rate at 25C

٤٠-٥٠

Softening Point ºC

٥٢-٦٠

Ductility 25C (cm)

Min 100

Flash PointºC

Min250

Solubility Disulfide %wt.

5/99

Stain Test

Negative

Wieght Loss by Heating %wt.

Max 2 /0

Wieght Loss by Heating، %

Max20

Road Construction Bitumen 60-70 Akam

Density

06/1-01/1

Penetration Rate at 25C

60-70

Softening Point ºC

49-56

Ductility 25C (cm)

Min 100

Flash PointºC

Min250

Solubility Disulfide %wt.

5/99

Stain Test

Negative

Wieght Loss by Heating %wt.

Max 2 /0

Wieght Loss by Heating، %

Max20

Road Construction Bitumen 60-70 Avije

Density

06/1-01/1

Penetration Rate at 25C

60-70

Softening Point ºC

49-56

Ductility 25C (cm)

Min 100

Flash PointºC

Min250

Solubility Disulfide %wt.

5/99

Stain Test

Negative

Wieght Loss by Heating %wt.

Max 2 /0

Wieght Loss by Heating، %

Max20

Road Construction Bitumen 60-70 Azar Bam

Density

06/1-01/1

Penetration Rate at 25C

60-70

Softening Point ºC

49-56

Ductility 25C (cm)

Min 100

Flash PointºC

Min250

Solubility Disulfide %wt.

5/99

Stain Test

Negative

Wieght Loss by Heating %wt.

Max 2 /0

Wieght Loss by Heating، %

Max20

Road Construction Bitumen 60-70 Bam Gostaran

Density

06/1-01/1

Penetration Rate at 25C

60-70

Softening Point ºC

49-56

Ductility 25C (cm)

Min 100

Flash PointºC

Min250

Solubility Disulfide %wt.

5/99

Stain Test

Negative

Wieght Loss by Heating %wt.

Max 2 /0

Wieght Loss by Heating، %

Max20

Road Construction Bitumen 60-70 Behbood Sanat

Density

1.01 -1.06

Penetration Rate at 25C

60-70

Softening Point ºC

49-56

Ductility 25C (cm)

Min 100

Flash PointºC

232 min

Solubility Disulfide %wt.

99.0 %

Stain Test

Negative

Viscosity@60°C

2000±400

Viscosity@135°C

300min

Road Construction Bitumen 60-70 Black Gold

specific gravity 25 DFG C

1 – 1.06

Penetration Rate at 25ºC "(mm/10)

60-70

Softening Point ºC

49-56

Ductility 25C (cm)

>100

Loss on Heating %wt.

>0.2

drop in pen after heating(%)

< 20%

Flash PointºC

250

Solubility in TCE %wt.

99.5%

Spot Test

Negative

wax content

< 2.0

Road Construction Bitumen 60-70 foolad sooren

Density

1010 – 1060

Penetration Rate at 25C

60-70

Softening Point ºC

49-56

Ductility 25C (cm)

Min 100

Flash PointºC

232

Solubility Disulfide %wt.

99.0

Stain Test

Negative

Wieght Loss by Heating %wt.

2.0

Wieght Loss by Heating، %

Max 20

Retained Penetration after (T.F.O.T)

54 min

Ductility, (25°C),5cm/min,cm after TFOT

50

Viscosity @60° C

1000 max

Road Construction Bitumen 60-70 Fouman Chimi Gostar

Density

1.01-1.06

Penetration Rate at 25C

60-70

Softening Point ºC

49-56

Ductility 25C (cm)

Min 100

Flash PointºC

Min250

Solubility Disulfide %wt.

99.5

Stain Test

Negative

Wieght Loss by Heating %wt.

Max 0/2

Wieght Loss by Heating، %

Max 20

Road Construction Bitumen 60-70 Isfahan Bitumen

Density

1010-1060

Penetration Rate at 25C

60-70

Softening Point ºC

49-56

Ductility 25C (cm)

> 100

Flash PointºC

>250

Solubility Disulfide %wt.

>99.5

Stain Test

Negative

Wieght Loss by Heating %wt.

Max 0.2

Wieght Loss by Heating، %

Max20

Road Construction Bitumen 60-70 Jey

Density

06/1-01/1

Penetration Rate at 25C

60-70

Softening Point ºC

49-56

Ductility 25C (cm)

Min 100

Flash PointºC

Min250

Solubility Disulfide %wt.

5/99

Stain Test

Negative

Wieght Loss by Heating %wt.

Max 2 /0

Wieght Loss by Heating، %

Max20